MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Description

Polyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Melt Flow 0.90 g/10 min
@Temperature 230 °C
0.90 g/10 min
@Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ASTM D785
Tensile Strength at Break 18.0 MPa2610 psiISO 527
Tensile Strength, Yield 27.6 MPa4000 psi2 in/min; ASTM D638
Elongation at Yield 30 %30 %ASTM D638
Flexural Modulus 1.45 GPa210 ksiASTM D790
Izod Impact, Notched 3.20 J/cm6.00 ft-lb/inASTM D256
Izod Impact, Unnotched NBNB-22°F; ASTM D256
Gardner Impact 14.47 J10.67 ft-lbASTM D3029
 43.4 J
@Temperature -28.9 °C
32.0 ft-lb
@Temperature -20.0 °F
ASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C235 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75
 62.8 °C145 °FASTM D648
 
Descriptive Properties
Thermal Oxidative StabilityPassASTM D3012, at 336 hrs, 150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Washington Penn PPH2CF2 Polypropylene, 20% Calcium Carbonate Reinforced
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Total PPH 3281 Polypropylene, Extrusion Grade
A. Schulman Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer

PASHU117 / 25081

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.