MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Inov Chem Doncool 103 CP/IP Base blend polyols
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Doncool 103 is blend polyols uses CP or CP/IP as blowing agent, which applies to refrigerators, freezers, and other insulation products. The characteristics of the products are as follows
1. Excellent flow ability, foam density distributes uniformity, low thermal conductivity
2. Excellent low temperature dimension stability and cohesiveness
3. Demould time 6~8 minutes

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 - 1.08 g/cc
Density 0.0240 - 0.0250 g/ccFree density, High pressure machine
 0.0250 - 0.0260 g/ccFree density, Manual mixing
 >= 0.0350 g/ccMold density; GB/T 6343
Viscosity 3000 - 4000 cPDynamic
Storage Temperature 10.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 0.150 MPaGB/T8813
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0220 W/m-K
@Temperature 15.0 °C
GB/T 3399
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 25.0 °CMaterial Temperature, Manual mixing
 20.0 - 25.0 °CMaterial Temperature, High pressure machine
Mold Temperature 35.0 - 40.0 °CManual mixing
 35.0 - 40.0 °CHigh pressure machine
Cure Time 70.0 - 100 secTack free time, High pressure machine
 100 - 120 secTack free time, Manual mixing
Gel Time 0.830 - 1.167 minHigh pressure machine
 1.25 - 1.416 minManual mixing
Shelf Life 6.00 Month
 
Descriptive Properties
AppearancePale yellow transparent liquid
Closed-cell rate=90%GB/T 10799
Cream time12-16 secManual mixing
 8-12 secHigh pressure machine
Dimensional stability=0.5%24h, -20?; GB/T8811
 =1.0%24h, 100?; GB/T8811
Hydroxyl value360-420 mgKOH/g
Recommended Ratio100Doncool 102
 12-14CP or CP/IP
 136-142Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM002 / 312531

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.