MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene™ Ultra UL 7840E Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Escorene Ultra UL 7840 is a high viscosity, 31.4% wt vinyl acetate copolymer that has good comparability with both hydrocarbon and natural tackifiers and is suitable for making hot melt adhesives, and sealants.  UL 7840E contains an additive package to improve pellet flowability and handling. 

Availability: Asia Pacific, North America, Latin America.  Additives: antiblock: no; slip: no;  thermal stabilizer: yes.  Applications: adhesives and sealants, industrial sealants, hot melt adhesives.  Form:  pellets.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 g/ccASTM D1505
Vinyl Acetate Content 31.4 %ExxonMobil Method
Melt Flow 43 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68
@Time 15.0 sec
ASTM D2240
Hardness, Shore D 14
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break >= 580 psiASTM D638
Elongation at Break >= 800 %ASTM D638
Flexural Modulus, 1% Secant 1900 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 142 °FPeak; ExxonMobil Method
Vicat Softening Point 118 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98948 / 238329

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.