MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Pressurfect CNG Austenitic Chromium-nickel Steel
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Pressurfect CNG is a dual grade certified (ASTM 316/316L) austenitic chromium-nickel steel with minimum 2.5% molybdenum and a low carbon content used for compressed natural gas (CNG) fuel systems. The grade is characterized by:
  • Excellent corrosion resistance in CNG environments
  • Excellent toughness
  • Excellent bendability
  • Excellent impact strength
Applications: Pressurfect CNG has been developed specifically for high-pressure fuel lines for compressed natural gas (CNG) systems in internal combustion engines.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B <= 90
Tensile Strength, Ultimate 515 - 690 MPaRm
Tensile Strength, Yield >= 220 MPa
@Strain 0.2 %
 >= 250 MPa
@Strain 1 %
 >= 150 MPa
@Strain 0.2 %,
Temperature 200 °C
 >= 165 MPa
@Strain 0.2 %,
Temperature 150 °C
 >= 180 MPa
@Strain 0.2 %,
Temperature 100 °C
 >= 180 MPa
@Strain 1 %,
Temperature 200 °C
 >= 195 MPa
@Strain 1 %,
Temperature 150 °C
 >= 200 MPa
@Strain 0.2 %,
Temperature 50.0 °C
 >= 215 MPa
@Strain 1 %,
Temperature 100 °C
 >= 230 MPa
@Strain 1 %,
Temperature 50.0 °C
Elongation at Break >= 40 %Based on L = 5.65 vS where L is the original gauge length and S the original cross-section area
Modulus of Elasticity 186 GPa
@Temperature 200 °C
 194 GPa
@Temperature 100 °C
 200 GPa
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
 17.0 µm/m-°C
@Temperature 30.0 - 200 °C
Specific Heat Capacity 0.485 J/g-°C
@Temperature 20.0 °C
 0.500 J/g-°C
@Temperature 100 °C
 0.515 J/g-°C
@Temperature 200 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 15.0 W/m-K
@Temperature 100 °C
 17.0 W/m-K
@Temperature 200 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 17.5 %
Manganese, Mn 1.7 %
Molybdenum, Mo 2.6 %
Nickel, Ni 13 %
Phosphorus, P <= 0.040 %
Silicon, Si 0.40 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5282 / 199846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.