MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Momentive Performance Materials GE Sealants & Adhesives Painter’s Pro Siliconized Acrylic Latex Caulk, White and Colors
Categories: Polymer; Thermoset; Silicone

Material Notes: Painter’s Pro Siliconized Acrylic Latex is an advanced grade caulk ideal for decorative paint projects. Painter’s Pro caulk is paint-friendly and low in odor. It guns out effortlessly, tools smoothly and cleans-up with soap and water. This formulation resists cracking and offers dependable adhesion and flexibility for interior and exterior projects. When fully cured, the caulk is resistant to stain-causing mold and mildew growth. Painter’s Pro Siliconized Acrylic Latex caulk creates durable seals that are resilient and tough for long-lasting professional results.

Features: Backed by a limited 50-year durability guarantee, Strong flexibility and adhesion – exceeds ASTM C-834 (0°C) requirements, Resists cracking-for long-lasting professional results, Paint-Friendly, will not fade, Cured caulk forms a waterproof seal, Low odor and low VOC (Meets CARB VOC Limits), Easy application, Soap and water clean-up.

Applications: Painter’s Pro Siliconized Acrylic Latex caulk can be used in a wide variety of interior and exterior applications, including trim, crown molding, baseboards, vents and around doors, windows.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³Uncured
Solids Content 79 - 83 %79 - 83 %By weight. Uncured.; ASTM C1250
Volatile Organic Compounds (VOC) Content <= 35 g/l<= 35 g/lUncured. Excluding water & exempt compounds
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4444ASTM 661
Elongation at Break 200 %200 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
Minimum Service Temperature, Air -26.1 °C-15.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 100 °C104 - 212 °FApplication Temp
Cure Time 1440 min24.0 hour3/16 inch bead size
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceSmooth & CreamyUncured
BaseAcrylic Latex
Carb Chem Curing VOC<1.5 wt.%Uncured. Non-Chem Curing.
Clean-upDamp Disposable Cloth
ColoralmondMAP210AD 12C, MAP205AD 5TG
 BlackMAP210BK 12C,
 Cool GrayMAP210CG 12C
 Dark BrownMAP210DB 12C
 Light BrownMAP210LB 12C
 Off WhiteMAP210OW 12C, MAP205OW 5TG
 Warm GrayMAP210WG 12C
 whiteMAP210WT 12C, MAP205WT 5TG
Consistency / SagPassed
Coverage Rate51 Lin. Ft.At 3/16" bead.
Crack ResistanceNone-passedASTM C792
Extension Recovery and AdhesionPassedGlass/Al. Clear. ASTM C736
Freeze/Thaw StabilityPassed / 5 Cycles at 0°FUncured. ASTM C731.
Heat Aging and Weight Lost Cracking, CaulkingPassed
Low Temperature FlexibilityPassedASTM C732
OdorSlight AcrylicUncured
Paint Ready Time30 minutes
PaintableLatex & Oil Based Paints
Peel StrengthPassedASTM C794, Dry
Stain/Color ChangePassedASTM C510
Water Ready24 hoursUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9948 / 265759

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.