MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elite® 5400 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: ELITE® 5400 enhanced polyethylene resin is a copolymer produced via INSITE® technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and optical properties for high strength blown film applications. In addition, ELITE 5400 resin offers a unique combination of low temperature seal initiation, higher modulus, and low blocking tendencies for automated packaging applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2 (a) when used unmodified and processed according to good manufacturing practices.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.916 g/cc
Melt Flow 1.0 g/10 min
@Load 2.16 kg
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 11.3 MPa
Film Tensile Strength at Yield, TD 11.2 MPa
Film Elongation at Break, MD 635 %
Film Elongation at Break, TD 662 %
Secant Modulus, MD 0.171 GPaFilm value
Secant Modulus, TD 0.1825 GPaFilm value
Elmendorf Tear Strength MD 630 gUnspecified film thickness
Elmendorf Tear Strength TD 770 gUnspecified film thickness
Dart Drop Test >= 830 g
Film Tensile Strength at Break, MD 53.9 MPa
Film Tensile Strength at Break, TD 51.7 MPa
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 102 °C
 
Optical PropertiesOriginal ValueComments
Haze 9.5 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 90.0 °CSeal Initiation temperature
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ELITE™ 5401G Enhanced Polyethylene Resin
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade
Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Borealis Borstar® FB2230 LLDPE for Film
Dow Elite® 5100 Linear Low Density Polyethylene

PDW472 / 34541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.