MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QSil 1000 43 Shore A, Addition Cure, Self-Bonding, One Part Siloxane Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 1000 is a one-component, self-bonding elastomer that has excellent adhesion to many substrates, and is designed for use in applications up to 300°C.

Key Features:

  • 100% solids - no solvents
  • Fast cure at elevated temperatures
  • Good abrasion resistance
  • Primerless adhesion to many substrates
  • Low viscosity
  • Material must be heat cured

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccUncatalyzed
Viscosity 38000 cPUncatalyzed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 43Cured 3 days at 150°C
Tensile Strength 425 psiCured 3 days at 150°C
Elongation at Break 180 %Cured 3 days at 150°C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °CCured 3 days at 150°C
Minimum Service Temperature, Air -60.0 °CCured 3 days at 150°C
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 min
@Temperature 200 °C
 40.0 min
@Temperature 150 °C
 60.0 min
@Temperature 100 °C
 
Descriptive Properties
ColorRedUncatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 702 DIFFUSION PUMP FLUID
Chemours Viton® GBLT-600S Fluoroelastomer Compound
Advanced Elastomer Systems Santoprene® 453-45 Thermoplastic Rubber
Radici Heraflex® HP 40-21-60 TPS-SEBS Thermoplastic Elastomer
Abatron AboCast/AboCure 8501-4/8501-4 High Temperature Resistant Epoxy

PACC2076 / 199464

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.