MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Schott PCE Photofilter Yellow 460
Categories: Ceramic; Glass; Optical; Filter

Material Notes:

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.56 g/cc0.0925 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 - 300 °C
5.00 µin/in-°F
@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 539 °C1000 °F
Softening Point 717 °C1320 °Fη=7.67.6 dPas
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5251.525
Transmission, Visible 89.9 %89.9 %VC
 90 %90 %VD65
 91 %91 %VA
 0.00 %
@Thickness 2.00 mm,
Wavelength 440 nm
0.00 %
@Thickness 0.0787 in,
Wavelength 440 nm
 45 %
@Thickness 2.00 mm,
Wavelength 460 nm
45 %
@Thickness 0.0787 in,
Wavelength 460 nm
 86 %
@Thickness 2.00 mm,
Wavelength 480 nm
86 %
@Thickness 0.0787 in,
Wavelength 480 nm
 90 %
@Thickness 2.00 mm,
Wavelength 500 nm
90 %
@Thickness 0.0787 in,
Wavelength 500 nm
 
Descriptive Properties
Colorimetry0.369D65, x
 0.37C, x
 0.435C, y
 0.443D65, y
 0.447A, y
 0.47A, x
Edge wavelengths455-465 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSGT9878 / 183131

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.