MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LNP Stat-Kon® DC-1006 EM MR BK8-250 Polycarbonate, Carbon Fiber Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes:
  • Features: Good Mold Release, Good Moldability, Electrically Conductive
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccMethod A; ASTM D792
Water Absorption 0.10 %at 24 hrs; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPaASTM D638
Tensile Strength, Yield 150 MPaASTM D638
Elongation at Break 1.8 %ASTM D638
Elongation at Yield 1.9 %ASTM D638
Tensile Modulus 19.6 GPaASTM D638
Flexural Strength 221 MPaASTM D790
Flexural Modulus 14.5 GPaASTM D790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.18 mm
ASTM D256
Izod Impact, Unnotched 4.85 J/cm
@Thickness 3.18 mm
ASTM D256
Izod Impact, Notched (ISO) 7.20 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 32.1 kJ/m²ISO 180
Falling Dart Impact 9.60 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 100 - 1.00e+6 ohmASTM D4496
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 144 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 141 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 304 - 327 °C
Mold Temperature 79.4 - 107 °C
Drying Temperature 121 °C
Dry Time 4 hour
Moisture Content 0.020 %Suggested
Back Pressure 0.172 - 0.345 MPa
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant
LNP Stat-Kon® DC-1002 EM FR BK8-115 Polycarbonate, Carbon Fiber Reinforcement
LNP Thermocomp® DF-1006 EM MR Polycarbonate, Glass Fiber Reinforcement
LNP Thermocomp® DF-1006 EP BK8-250 Polycarbonate, Glass Fiber Reinforcement

PZLNP1303 / 51385

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.