MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Cristal™ Renew 401-50, Natural Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Cristal™ Renew 401-50 copolyester is a high flow product that contains mold release for ease of ejection. It is designed and engineered specifically for cosmetics packaging applications. With its unsurpassed color and clarity and an unmatched ability to mold thick parts with improved gate aesthetics, Cristal 401-50 Renew is clearly a well-suited copolyester for premium cosmetics packaging. Other outstanding features of Cristal™ Renew 401-50 copolyester are excellent chemical resistance, high gloss, and improvements in processing such as faster cycle times, and lower scrap rates. Cristal Renew 401-50 is also ideally suited for two-shot molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow characteristics.

Applications

  • Bottles-color cosmetics pkg
  • Color cosmetics packaging
  • Jars-skin care pkg
  • Personal care & cosmetics packaging
  • Skin care packaging
Key Attributes
  • Ability to mold thick parts
  • Ease of processing
  • Easy to extrude, cut, decorate, and seal
  • Excellent clarity and color
  • Excellent colorability
  • Good impact strength
  • Good stiffness
  • High gloss appearance
  • Improved gate aesthetics
  • Readily fill intricate molds
  • Toughness

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.00200 - 0.00500 cm/cm
@Thickness 3.17 mm
0.00200 - 0.00500 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength at Break 20.0 MPa2900 psiISO 527
 24.0 MPa3480 psiASTM D638
Tensile Strength, Yield 50.0 MPa7250 psiISO 527
 50.0 MPa7250 psiASTM D638
Elongation at Break 39.0 %39.0 %ISO 527
 44.0 %44.0 %ASTM D638
Elongation at Yield 4.30 %4.30 %ISO 527
 4.40 %4.40 %ASTM D638
Tensile Modulus 2.027 GPa294.0 ksiISO 527
 2.036 GPa295.3 ksiASTM D638
Flexural Yield Strength 66.0 MPa9570 psiASTM D790
Flexural Modulus 1.808 GPa262.2 ksiASTM D790
Izod Impact, Notched  0.440 J/cm
@Temperature -40.0 °C
0.824 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 1.03 J/cm
@Temperature 23.0 °C
1.93 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C154 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C142 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 0.400 %0.400 %ASTM D1003
Transmission, Visible 91.8 %91.8 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 205 - 240 °C401 - 464 °F
Mold Temperature 16.0 - 38.0 °C60.8 - 100 °F
Drying Temperature 65.0 °C149 °F
Dry Time 8.00 hour8.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4060 / 323683

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.