MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
J6 Polymers JFOAM™ A-206 Engineered Specialty Foam
Categories: Other Engineering Material

Material Notes: JFoam™ A-206 is used in random fabrication, antenna filling, structural panels, and aircraft control sections. A-206 is not to be used where cross section is greater than three inches. A-206 has a small uniform cell structure and a low viscosity at pour point

Information provided by J6 Polymers LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.00 lb/ft³Molded
Viscosity 42 cP
@Temperature 48.9 °C
T Component
 48 cP
@Temperature 43.3 °C
T Component
 59 cP
@Temperature 37.8 °C
T Component
 75 cP
@Temperature 32.2 °C
T Component
 100 cP
@Temperature 26.7 °C
T Component
 138 cP
@Temperature 21.1 °C
T Component
 9900 cP
@Temperature 48.9 °C
R Component
 10750 cP
@Temperature 43.3 °C
R Component
 32000 cP
@Temperature 37.8 °C
R Component
 56000 cP
@Temperature 32.2 °C
R Component
 98000 cP
@Temperature 26.7 °C
R Component
 186000 cP
@Temperature 21.1 °C
R Component
Outgassing - Total Mass Loss 2.0 %
Collected Volatile Condensable Material 0.90 %
Storage Temperature 65.0 - 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 190 psi
Tensile Stress at Strain 110 psi
@Strain 2 %
Modulus of Elasticity 5.60 ksi
Modulus of Rigidity 2.00 ksi
Compressive Strength 150 psi
Shear Strength 130 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.12
@Frequency 9.375e+9 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.280 BTU-in/hr-ft²-°FK-Factor
Maximum Service Temperature, Air 250 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 93.3 °C
Shelf Life 12.0 Month
 
Descriptive Properties
Mixing Ratio0.49T Component TDI Prepolymer
 0.51R Component Water Blown Polyol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
J6 Polymers JFOAM™ A-204 Engineered Specialty Foam
J6 Polymers JFOAM™ A-210 Engineered Specialty Foam
J6 Polymers JFOAM™ AC-555 Engineered Specialty Foam
J6 Polymers JFOAM™ G-304 Engineered Specialty Foam
Lendell Supersoft Foams

PJSIX002 / 190929

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.