Polypropylene PPH 7089 is a narrow molecular weight distribution homopolymer polypropylene, with anti-gas fading stabilization. Polypropylene PPH 7089 is intended for the extrusion of fibers with the spunbond technology. It is also suitable for extrusion of continuous filaments (CF). Information provided by Total Petrochemicals. |