MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Daplen™ EG066AI Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Daplen EG066AI is an elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness.

Typical characteristics:

  • High crystallinity
  • High flowability
  • UV stabilized
  • Good surface aesthetics
Applications:
  • Center consoles
  • Interior trims
  • Door panels and pockets
  • Pillar trims
Daplen EG066AI has been developed especially for the car industry to be used in automotive interior parts.

Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Melt Flow 22.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
22.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 20.0 MPa2900 psi50 mm/min; ISO 527-2
Flexural Modulus 1.00 GPa145 ksi2 mm/min; ISO 178
Charpy Impact, Notched 0.800 J/cm²
@Temperature -20.0 °C
3.81 ft-lb/in²
@Temperature -4.00 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C181 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 80.0 °C104 - 176 °F
 210 - 250 °C410 - 482 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
 
Descriptive Properties
Flow front speed100 - 200 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9700 / 323057

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.