BrushForm® 96 Strip is a high-performance, heat treatable spinodal copper nickel tin alloy designed to provide optimal formability and strength characteristics in conductive spring applications such as electronic connectors, switches, and sensors. It is available in both pre-heat treated (mill hardened) and heat treatable (age hardenable) forms.Information supplied by Materion. |