MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCast/AboCure 8502-1 Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-viscosity, flexibilized resin with long pot life. It is also available in colors and in filled form. It is easy to use and its shelf life is virtually indefinite.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.70 lb/gal
Water Absorption 0.30 - 0.40 %
@Time 864000 sec
Viscosity 46 cP
@Temperature 65.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85
Tensile Strength, Ultimate 9800 psi
Elongation at Break 1.7 %
Elongation at Yield 4.7 %
Tensile Modulus 850000 psi
Flexural Strength 9400 psi
Flexural Modulus 300000 psi
Compressive Yield Strength 15000 psi
Compressive Modulus 485000 psi
Izod Impact, Notched 0.600 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.50e+15 ohm-cmCond. C (96 hrs/23°C/96% rel. humidity)
 5.10e+15 ohm-cmCond. A (as received)
Surface Resistance 2.70e+14 ohmCond. C
 2.80e+14 ohmCond. A
Dielectric Constant 3.23
@Frequency 1e+6 Hz
Cond. A (as received)
 3.32
@Frequency 1e+6 Hz
Cond. D (48 hrs. in dist. H2O at 50°C)
 3.44
@Frequency 1000 Hz
Cond. A (as received)
 3.47
@Frequency 60 Hz
Cond. A (as received)
 3.93
@Frequency 1000 Hz
Cond. D (48 hrs. in dist. H2O at 50°C)
 4.16
@Frequency 60 Hz
Cond. D (48 hrs. in dist. H2O at 50°C)
Dissipation Factor 0.0070
@Frequency 1000 Hz
Cond. A (as received)
 0.0079
@Frequency 60 Hz
Cond. A (as received)
 0.026
@Frequency 1e+6 Hz
Cond. A (as received)
 0.032
@Frequency 1000 Hz
Cond. D (48 h. in dist. H2O at 50°C)
 0.045
@Frequency 1e+6 Hz
Cond. D (48 h. in dist. H2O at 50°C)
 0.055
@Frequency 60 Hz
Cond. D (48 h. in dist. H2O at 50°C)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 65.0 µm/m-°C
Thermal Conductivity 0.000400 - 0.000480 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 49.0 °CDeflection Temp at unknown load
 
Processing PropertiesOriginal ValueComments
Cure Time 120 - 180 min
@Temperature 150 - 160 °C
 960 min
@Temperature 95.0 °C
Pot Life 420 min
@Temperature 65.0 °C
 2880 min
@Temperature 20.0 °C
 
Descriptive Properties
Deflection at Break0.53 in.
Parts by Weight (pbw)100AboCast
 88AboCure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman Araldite GY 281 Bisphenol F Epoxy Resin
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Epoxy, Cast, Unreinforced
Abatron AboCast 7703-21/AboCure 7703-23 (C) Epoxy Adhesive and Casting Compound
304 Stainless Steel

PABC876 / 107860

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.