Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Filler/Reinforcement: Mineral, 40% Filler by Weight Features: Good Heat Resistance Uses: Automotive Applications; Automotive Interior Parts; Consumer Applications; Engineering Parts; Household Goods; Hydraulic Applications; Industrial Applications; Pneumatic Applications; Power/Other Tools; Sporting Goods Agency Ratings: NSF STD-61 RoSH Compliance: RoSH Compliant Forms: Granules Processing Method: Injection Molding Information provided by EMS-Grivory |