MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ineos Nova S-7600MG Compact Polystyrene Microgranulates  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: High impact polystyrene Microgranulates, having a diameter of 0.8 -1.0 mm, especially useful for compounding and extrusion applications. Due to the very high viscosity and the absence of weakener, end-products of compounding or extruding are very hard and stiff.

All mechanical properties measured under standard conditions 50% RH and 23°C.

Information provided by NOVA Chemicals.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³DIN 53479
Water Absorption <= 0.10 %<= 0.10 %DIN 53495
Melt Flow 2.5 g/10 min2.5 g/10 minDIN 53735/ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 28.0 MPa4060 psiDIN 53455
Elongation at Break 30 %30 %DIN 53455
Modulus of Elasticity 1.50 GPa218 ksiDIN 53457
Flexural Yield Strength 24.0 MPa3480 psiDIN 53452
Flexural Modulus 1.40 GPa203 ksiDIN 53457/ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²Low Temp; DIN 53453
 8.00 kJ/m²3.81 ft-lb/in²DIN 53453/ISO 179
Izod Impact, Unnotched (ISO) 6.00 kJ/m²2.86 ft-lb/in²DIN 53453
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.160 W/m-K1.11 BTU-in/hr-ft²-°FDIN 52612
Vicat Softening Point 96.0 °C205 °FDIN 53460

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVA097 / 54998

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.