MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
AISI 1141 Steel, cold finished round (19-38 mm)
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: End products from this steel are often cyanided or carbonitrided. Can also be flame and induction hardened, and oil quenched after case hardening.

Key Words: UNS G11410
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 223
Hardness, Knoop 246Converted from Brinell
Hardness, Rockwell B 96Converted from Brinell
Hardness, Rockwell C 18
Hardness, Vickers 235Converted from Brinell
Tensile Strength, Ultimate 772 MPa
Tensile Strength, Yield 655 MPa
Elongation at Break 16 %in 50 mm
Reduction of Area 40 %
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Typical For Steel
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000170 ohm-cm
@Temperature 20.0 °C
condition of specimen unknown
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.472 J/g-°CTypical steel
Thermal Conductivity 49.8 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.37 - 0.45 %
Iron, Fe 97.73 - 98.2 %As remainder
Manganese, Mn 1.35 - 1.65 %
Phosphorus, P <= 0.040 %
Sulfur, S 0.080 - 0.13 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1141 Steel, as cold drawn, 50-75 mm (2-3 in) round
AISI 1141 Steel, as rolled
AISI 1141 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
AISI 1141 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1141 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round

M1141F / 7237

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.