MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Martensitic
Categories: Metal; Ferrous Metal; Martensitic

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Martensitic". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 6.45 - 7.89 g/ccAverage value: 7.72 g/cc Grade Count:110
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 160 - 700Average value: 327 Grade Count:41
Hardness, Rockwell B 80.0 - 109Average value: 94.8 Grade Count:22
Hardness, Rockwell C 22.0 - 68.0Average value: 46.9 Grade Count:69
Hardness, Vickers 200 - 1100Average value: 526 Grade Count:19
Tensile Strength, Ultimate 345 - 2350 MPaAverage value: 1180 MPa Grade Count:120
Tensile Strength, Yield 205 - 1910 MPaAverage value: 961 MPa Grade Count:103
Elongation at Break 2.00 - 34.0 %Average value: 13.7 % Grade Count:88
Elongation at Yield 2.00 - 40.0 %Average value: 12.9 % Grade Count:6
Reduction of Area 2.00 - 67.0 %Average value: 43.0 % Grade Count:28
Modulus of Elasticity 77.0 - 310 GPaAverage value: 201 GPa Grade Count:60
Compressive Yield Strength 745 - 3120 MPaAverage value: 2240 MPa Grade Count:3
Bulk Modulus 166 GPaAverage value: 166 GPa Grade Count:7
Poissons Ratio 0.230 - 0.346Average value: 0.278 Grade Count:21
Fatigue Strength 400 - 621 MPaAverage value: 541 MPa Grade Count:3
Machinability 30.0 - 65.0 %Average value: 53.8 % Grade Count:6
Shear Modulus 62.1 - 86.5 GPaAverage value: 78.0 GPa Grade Count:21
Izod Impact Unnotched 13.6 - 244 JAverage value: 79.1 J Grade Count:5
Charpy Impact 6.00 - 169 JAverage value: 51.9 J Grade Count:17
Bend Radius, Minimum 3.00 - 9.00 tAverage value: 5.33 t Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000600 - 0.0000980 ohm-cmAverage value: 0.0000654 ohm-cm Grade Count:39
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.02 - 16.8 µm/m-°CAverage value: 11.3 µm/m-°C Grade Count:53
Specific Heat Capacity 0.460 - 0.460 J/g-°CAverage value: 0.460 J/g-°C Grade Count:35
Thermal Conductivity 14.0 - 32.3 W/m-KAverage value: 24.5 W/m-K Grade Count:29
Melting Point 1120 - 1530 °CAverage value: 1430 °C Grade Count:12
Solidus 1400 - 1480 °CAverage value: 1420 °C Grade Count:10
Liquidus 1470 - 1530 °CAverage value: 1490 °C Grade Count:10
Maximum Service Temperature, Air 371 - 649 °CAverage value: 490 °C Grade Count:3
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 593 - 899 °CAverage value: 763 °C Grade Count:3
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.0400 - 1.50 %Average value: 0.948 % Grade Count:13
Boron, B 0.00300 - 0.0100 %Average value: 0.00475 % Grade Count:4
Carbon, C 0.0200 - 3.90 %Average value: 0.376 % Grade Count:134
Chromium, Cr 0.0500 - 18.0 %Average value: 12.9 % Grade Count:136
Copper, Cu 0.100 - 5.00 %Average value: 3.20 % Grade Count:33
Iron, Fe 56.2 - 96.0 %Average value: 80.6 % Grade Count:121
Manganese, Mn 0.150 - 2.00 %Average value: 0.764 % Grade Count:117
Molybdenum, Mo 0.0270 - 4.00 %Average value: 1.41 % Grade Count:62
Nb + Ta 0.150 - 0.450 %Average value: 0.295 % Grade Count:21
Nickel, Ni 0.200 - 8.50 %Average value: 3.27 % Grade Count:79
Niobium, Nb (Columbium, Cb) 0.0600 - 3.00 %Average value: 0.443 % Grade Count:16
Nitrogen, N 0.0150 - 0.170 %Average value: 0.0767 % Grade Count:9
Phosphorus, P 0.0100 - 0.0600 %Average value: 0.0316 % Grade Count:67
Silicon, Si 0.0500 - 3.50 %Average value: 0.705 % Grade Count:114
Sulfur, S 0.00100 - 0.150 %Average value: 0.0241 % Grade Count:67
Tungsten, W 0.100 - 3.50 %Average value: 1.27 % Grade Count:8
Vanadium, V 0.0200 - 9.00 %Average value: 1.65 % Grade Count:19

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Carbon Steel
Overview of materials for Austenitic
Overview of materials for Stainless Steel
Overview of materials for High Carbon Steel
Overview of materials for Low Alloy Steel

M01020 / 81727

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.