MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Incoloy alloy 802 Superalloy
Categories: Metal; Ferrous Metal

Material Notes: Annealed

Al0.6-Cr21-Fe46-Ni32.5-Ti0.75

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.82 g/cc
 
Mechanical PropertiesOriginal ValueComments
Rupture Strength 24.0 MPa
@Temperature 980 °C,
Time 3.60e+6 sec
 48.0 MPa
@Temperature 980 °C,
Time 360000 sec
 186 MPa
@Temperature 650 °C,
Time 3.60e+6 sec
 262 MPa
@Temperature 650 °C,
Time 360000 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.60 %
Chromium, Cr 21 %
Iron, Fe 46 %
Nickel, Ni 32.5 %
Titanium, Ti 0.75 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Incoloy 840 Superalloy
Haynes 556® alloy, 50% cold reduction
Haynes 556® alloy, 0% cold reduction
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Haynes 263® alloy, cold rolled sheet, solution treated and aged

NZ97108 / 200170

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.