MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 205 FR XB Nylon 6/6 (PA), Glass Fiber - Flame Retardant - RoHS Compliant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccASTM D 792
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0015 - 0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 145 MPa21000 psiASTM D 638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ASTM D 638
Tensile Modulus 10.0 GPa1450 ksiASTM D 638
Flexural Strength 234 MPa34000 psiASTM D 790
Flexural Modulus 10.3 GPa1500 ksiASTM D 790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.20 mm
1.30 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 7.47 J/cm
@Thickness 3.20 mm
14.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 29.5 kV/mm750 kV/inShort Term; In Oil; ASTM D 149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 249 °C480 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 232 °C450 °FASTM D 648
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
UL 94
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
UL 94
Glow Wire Ignition Temperature 850 °C
@Thickness 0.800 mm
1560 °F
@Thickness 0.0315 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 299 °C530 - 570 °F
Mold Temperature 65.6 - 107 °C150 - 225 °F
Drying Temperature 79.4 °C
@Time 14400 sec
175 °F
@Time 4.00 hour
Moisture Content 0.20 %0.20 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 124 MPa10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 205D HS  Nylon 6/12 (PA 6/12) Glass Fiber 30% - Heat Stable
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced
RTP Company RTP 203 FR XB Nylon 6/6 (PA), Glass Fiber - Flame Retardant - RoHS Compliant
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM)

PQZTA21632 / 159262

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.