MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Primex Plastics Prime ABS Film-X 100 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Prime ABS Film-X 100 is a Prime ABS substrate with a UV and chemical resistant film. It is available in high gloss with a good DOI or low gloss.

Applications: Prime ABS Film-X has a wide variety of possible exterior applications from side pillars, spoilers, side molding. It is ideal for any exterior application requiring a very high gloss or dull finish with UV and chemical resistance.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Melt Flow 6.0 g/10 min6.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 37.9 MPa5500 psiASTM D638
Film Tensile Strength at Yield, TD 36.5 MPa5300 psiASTM D638
Flexural Modulus 1.89 GPa274 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 87.8 µm/m-°C48.8 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C200 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.7 °C179 °FASTM D648
Flammability, UL94 HB
@Thickness >=2.69 mm
HB
@Thickness >=0.106 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIM010 / 278481

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.