MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc 50-3253FR Flame Retardant Thermally Conductive Epoxy Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Description: 50-3253FR Potting and Encapsulating Compound has been formulated to meet the stringent non-burning requirements of UL 94 V-0. This medium viscosity system offers high thermal conductivity, low shrinkage, low exotherm, and outstanding electrical insulation properties. The high thermal conductivity helps extend the life of assemblies by quickly dissipating heat away from critical components. 50-3253FR is designed for ease of use. It has a convenient 1:1 mix ratio. Typical applications for the 50-3253FR include potting and encapsulating power supplies, transformers, batteries, coils, insulators, sensors, etc. The 50-3253FR is an excellent choice for applications that require a flame retardant compound with high thermal conductivity.

Features:

  • Thermally conductive
  • Easy 1:1 ratio
  • Shock and vibration resistant
  • Flame Retardant cuitry
Benefits:
  • Protects electronics by quickly transferring heat
  • Ideal for use with meter mix dispense equipment
  • Will not damage electronic components
  • Meets UL94V-0 non-burning requirements

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccHardener
 1.60 g/ccResin
Viscosity 60000 cPResin
 60000 cPMixed
 64000 cPHardener
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55
@Temperature 75.0 °C
 80
@Temperature 25.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.60e+13 ohm-cm
Dielectric Constant 5.0
@Frequency 100 Hz
Dielectric Strength 485 V/mil
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2.16 W/m-K
Maximum Service Temperature, Air 155 °C
Minimum Service Temperature, Air -65.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 65.0 °C
 30.0 min
@Temperature 100 °C
 24.0 - 48.0 hour
@Temperature 25.0 °C
Pot Life 100 min
@Load 0.100 kg
 
Descriptive Properties
ColorBeigeHardener
 BlackMixed
 BlackResin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX062 / 316739

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.