MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Kendall® Extended Bearing Life (EBL) Grease NLGI Grade 0
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Kendall® Extended Bearing Life (EBL) Grease is a semifluid, extreme-pressure polyurea grease specially developed for the lubrication of wheel bearings on non-driven truck trailer axles equipped with oil seals. It is formulated to help optimize service intervals and reduce operating costs by providing effective lubrication and cooling of wheel bearings exposed to the prolonged high operating temperatures of over-the-road applications. EBL Grease is manufactured with high-quality base oils and a non-soap, polyurea thickener. It is fortified with extreme-pressure additives and rust and oxidation inhibitors to provide excellent wear protection, protection against rust and corrosion, and long service life. It has excellent thermal stability at high temperatures and excellent pumpability at low temperatures for use over a wide range of operating temperatures. It has excellent compatibility with elastomer seals and is resistant to water washout.

Applications:

  • Wheel bearings of non-driven trailer axles equipped with oil seals
Features/Benefits:
  • Excellent oxidation resistance and thermal stability at high temperatures
  • Excellent pumpability at low temperatures
  • Good load-carrying capacity
  • Protects against rust and corrosion
  • Resists water washout
  • Excellent seal compatibility
  • Formulated for extended service life

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.35 lb/gal
Viscosity Measurement 98Index
Saybolt Viscosity at 100°F 575 SUS
Saybolt Viscosity at 210°F 68 SUS
Kinematic Viscosity at 40°C (104°F) 110 cSt
Kinematic Viscosity at 100°C (212°F) 12 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.400 mmScar Diameter; ASTM D2266
Penetration P(60), 1/10 mm 355 - 385ASTM D217
Timken Test 40.0 lbASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 149 °C
Minimum Service Temperature, Air -29.0 °C
Dropping Point 204 °C
 
Descriptive Properties
ColorLight Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5325 / 198578

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.