MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes:

Characteristics:

  • High shock resistant ( high impact strength )
  • High Mechanical Strength
  • High Dielectric Strength
  • High Electrical Insulation
  • Color- pale brown
  • Medium flow
  • Applications:

  • Electric motor end shield
  • Electrical panel components to withstand high impact
  • High mechanical strength laminated sheets
  • Moulded items to withstand high mechanical shock
  • Automotive lamp caps
  • Moudlings exposed to warm & humid climate
  • Moulding exposed to low intensity flame and spark, etc.
  • Grinding disc centres
  • Castors
  • Gas meter parts
  • Gas regulator knobs, etc.
  • Information provided by Amity Thermosets Limited

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.85 - 2.10 g/ccMolding; IS 867-1963
    Water Absorption 0.050 - 0.20 %IS 13411-1993
    Linear Mold Shrinkage 0.00050 - 0.0015 cm/cmIS 13411-1992
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 90.0 - 106 MPa5 mm/min.; IS 867-1963
    Shear Strength 120 - 180 MPa2mm/min.; IS 867-1963
    Izod Impact, Notched 1500 - 2000 J/mIS 13411-1992
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity >= 1.00e+12 ohm-cmIS 3396-1979
    Surface Resistance >= 1.00e+11 ohmIS 3396-1979
    Dielectric Strength >= 8.00 kV/mm
    @Temperature 90.0 °C
    IS 2584-1963
    Comparative Tracking Index >= 175 V2824-1975
     
    Processing PropertiesOriginal ValueComments
    Mold Temperature 160 - 180 °C
    Injection Pressure 15.68 - 34.3 MPaMold Pressure
    Cure Time 80.0 - 110 secper mm
    Shelf Life 4.00 Month10-25°C

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Overview of materials for Phenolic/Glass Fiber SMC
    Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
    Overview of materials for Phenolic, Novolac, Glass Filled
    Bakelite® PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
    Bakelite® PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength

    PAMITY32 / 24060

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.