Features: Replaces dense castable burner blocksLightweight Excellent insulator/thermal shock resistant High mechanical abuse resistance Variety of sizes/attachment systems Low heat storage Cost effective Applications: EDC (Ethylene Dichloride) linings VCM (Vinyl Chloride Monomer) liningsEthylene heaters and reformersInformation provided by Thermal Ceramics Data has not been recently verified. Please contact manufacturer for current information. |