Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for thin wall, architectural glazing and sealing applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion or thermoforming. It is polyolefin based and completely recyclable. Key Features: - Recommended for glazing and sealing applications.
- Designed for extruding thin sections with excellent definition (down to 0.33 mm [0.023"] radius) Long runs with minimal build-up of material on screen packs or narrow die sections.
- Recommended for applications requiring excellent ozone resistance.
- Recommended for applications requiring excellent flex fatigue resistance.
- EU and China RoHS compliant.
Processing Method: Coextrusion, Profile Extrusion, Thermoforming, Extrusion and Sheet ExtrusionAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America Processing Method: Coextrusion, Profile Extrusion, Thermoforming, Extrusion and Sheet Extrusion Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical. |