MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Silfoam® SD 168 Silicone Antifoam Agent
Categories: Fluid

Material Notes: Product description: SILFOAM® SD 168 is a very compatible, anhydrous antifoam agent that is easily disperable. SILFOAM® SD 168 is intended for incorporation into non-structured liquid detergents for foam control and polymer dispersions (latices) in order for deaeration.

Application: By virtue of its chemical structure, SILFOAM® SD 168 is capable of regulating surfactant-based formulations, in particular liquid detergents; undesirable side effects such as incompatibility, insufficient alkali resistance or rapid loss of effect are significantly reduced. Its principal areas of application are in non-structured liquid detergents and cleaners. When introduced into dispersions SILFOAM® SD 168 shows relatively good compatibility with the polymer film and high efficiency during storage, especially at higher temperatures. Typical applications of SILFOAM® SD 168 are all kinds of dispersions, especially for the construction industry, masonry paints and adhesives.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9637 g/cc
@Pressure 0.1013 MPa
DIN 12791
Brookfield Viscosity 400 cPdynamic, spindle 2/ 50 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 75.0 °CISO 2719
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.42 - 1.43DIN 51423
 
Descriptive Properties
Active ingredients (%)100
Appearanceslightly opaque, colorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9445 / 204974

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.