MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Manganese Bronze, UNS C86200, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Die, Investment, Permanent Mold, and Sand.

Applications: Marine castings, gears, gun mounts, bushings and bearings.

Classified under: Manganese and leaded manganese bronze alloys. ASTM B584; formerly ASTM B147-8B

As cast values below are for sand casting. Alloy does not respond to heat treating

Key Words: High Strength Manganese Bronze, high strength yellow brass, CA 862, ASTM B30, ASTM B271, ASTM B505, ASTM B584; ASTM B147-8B, FED QQ-C-390, FED QQ-C-523, MIL-C-22087 (composition 9), MIL-C-11866 (composition 20), MIL-C-22229 (composition 9), Ingot code no. 423
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 180
Tensile Strength, Ultimate 655 MPa
Tensile Strength, Yield 330 MPa
Elongation at Break 20 %In 50 mm
Modulus of Elasticity 105 GPa
Compressive Strength 345 MPaat permanent set of 0.1%
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
Izod Impact 16.0 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00002298 ohm-cm
@Temperature 20.0 °C
7.5% IACS
Magnetic Permeability 1.2416 kA/m field strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 µm/m-°C
@Temperature 20.0 - 260 °C
Specific Heat Capacity 0.376 J/g-°C
Thermal Conductivity 35.0 W/m-K
@Temperature 20.0 °C
Melting Point 900 - 940 °C
Solidus 900 °C
Liquidus 940 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 260 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.0 - 7.5 %
Copper, Cu 60 - 68 %
Iron, Fe 2.0 - 4.0 %
Lead, Pb <= 0.20 %
Manganese, Mn 2.5 - 5.0 %
Nickel, Ni <= 1.0 %
Tin, Sn <= 0.20 %
Zinc, Zn 26 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Manganese Bronze, UNS C86300, Copper Casting Alloy
Manganese Bronze, UNS C86100, Copper Casting Alloy
Leaded High-Strength Yellow Brass, UNS C86400, Copper Casting Alloy
High-Strength Yellow Brass, UNS C86500, Copper Casting Alloy
Manganese Bronze A, UNS C67500

MC86200b1 / 11913

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.