MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Arcol® E-919 Polyether Polyol
Categories: Polymer; Thermoset

Material Notes: Characterization: Arcol E-919 polymer polyol is a 29% total solids polymer polyol for increasing the load bearing capacities of HR foams.

Properties / Applications: Arcol E-919 polymer polyol is a 29% total solids polymer polyol for increasing the load bearing capacities of HR foams. It is based on a reactive, EO capped, triol of approximately 1,600 equivalent weight. Arcol E-919 offers good processing and formulating latitude over a wide range of dilutions with various HR base polyols. This enables the user to produce a broad range of high quality HR foam grades. As with any product, use of Arcol E-919 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Warning: The oxidation inhibitor components in Arcol E-919 polyol may not provide adequate protection against scorch and/or fire in the production of lower density foams by a slabstock or box machine process. If used in the production of such foam, the user needs to insure that adequate oxidation inhibitor is added (through diluent polyol or direct addition) to safely produce the intended foam grades.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.045 g/cc1.045 g/cc
Bulk Density 1.04 g/cc0.0376 lb/in³
Viscosity 2500 cP2500 cP
Storage Temperature 20.0 - 60.0 °C68.0 - 140 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.060 %<= 0.060 %
 
Descriptive Properties
Hydroxyl number23.4-27.4 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Arcol® F-1080 Polyol
Covestro Arcol® F-3040 Polyol
Covestro Arcol® F-3022 Polyol
Covestro Arcol® F-1522 Polyether Polyol
Covestro Arcol® E-434 Polyether Polyol

PCOVEST0020 / 201803

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.