MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF N-Butanol
Categories: Fluid; Solvent

Material Notes: Formula: C4H10O

CAS: 71-36-3

Description: n-Butanol is a clear, mobile, neutral liquid with a characteristic odor. It is miscible with all common solvents, e.g., alcohols, ketones, aldehydes, ethers, glycols, and aromatic and aliphatic hydrocarbons, but is only sparingly soluble in water

Applications: A large part of the n-Butanol produced is converted into derivatives(primarily esters) for use as solvents in the coatings industry. n-Butanol is an eminently suitable solvent for acid-curable lacquers and baking finishes derived from urea (Plastopal), melamine (Luwipal), or phenolic resins. Some butyl esters of dicarboxylic acids, phthalic anhydride, and acrylic acid are established plasticizers for plastics, rubber mixes, and dispersions. The most important are dibutyl phthalate (DBP), benzylbutyl phthalate (BBP), and butyl acrylate. Dibutylsebacate (DBS) and dibutyl azelate(DBZ) are of subordinate importance. The corresponding adipate is too volatile to be a plasticizer and is therefore of no practical significance in these applications. The applications in which normal butane can be used are as follows: solvent for dyes, e.g. in printing inks; extractant in the production of drugs and natural substances such as antibiotics, hormones, vitamins, alkaloids and camphor; additive in polishes and cleaners, e.g. floor cleaners and stain removers; solubilizer in the textile industry, e.g. additive in spinning baths or carrier for coloring plastics; additive in deicing fluids; gasoline additive (antiicing); mobile phase in paper and thinlayer chromatography; humectant for cellulose nitrate; feedstock for the production of glycol ethers (in reactions with ethylene or propylene oxide); starting material for various butyl monocarboxylates, e.g. butyl acetate and butyl butyrate, that are widely used as solvents; and feedstock for the production of flotation aids, e.g. butyl xanthate

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.810 - 0.813 g/cc
Molecular Weight 74.1 g/mol
 
Thermal PropertiesOriginal ValueComments
Distillation Temperature 117 - 118 °C
@Pressure 0.101 MPa
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %ASTM D1364
 
Descriptive Properties
Acidity, as HCI0.003as acetic acid, ASTM D1613
Assay>99.8%
Color<5ASTM D1209

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Glacial Acrylic Acid
BASF Isobutanol
BASF Butyl Acrylate
BASF 2-Ethylhexanol
LG Chemical 2-EH 2-Ethyl Hexanol

PBASG0890 / 132523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.