MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Starplex® Premium NLGI Grade 1
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Texaco Starplex Premium delivers value through:
  • Continuous high temperature stability up to 325°F.
  • Excellent corrosion and wear protection.
  • Excellent water resistance.
  • Extended relubrication intervals because of its excellent resistance to water washout.

Texaco Starplex Premium is a lithium complex grease, formulated with a high viscosity base oil and special additives, including polymers to impart extreme pressure characteristics as well as corrosion, wear oxidation and water wash out protection.

Texaco Starplex Premium provides an alternative for high temperature applications. The high viscosity base oils contained in this product serve to minimize friction between moving parts and boost lubrication performance over a wide temperature range.

Texaco Starplex Premium is recommended for use in applications with temperatures up to 325°F. It is ideally suited for lubrication where water washout is an issue.

Texaco Starplex Premium is ideal for a wide variety of applications across several industries, including:

  • Paper and Forest Products — This lubricant is superior for severe service applications such as: sludge press bearings, lime kilns, pumps, woodyard heavy equipment, Doctor oscillator bearings, felt roll bearings, pulp refiner bearings, rope sheaves, and exhaust fan bearings.
  • Mining — Texaco Starplex Premium is particularly recommended for:
    • Mining operations that involve extreme pressure applications requiring good low temperature pumpability. Applications include: pins and bushings on buckets and loaders, shaker screens, crushers, and conveyors
    • The lowest temperature mining applications
    • Automatic lubricating systems in onboard shovels, trucks, and other mobile equipment.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 221937; MSDS Number: 9021

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9090Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 2537 SUS2537 SUSSee Note 3.
Saybolt Viscosity at 210°F 147 SUS147 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 475 cSt475 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 30 cSt30 cStSee Note 3.
 
Mechanical PropertiesMetricEnglishComments
Penetration P(60), 1/10 mm 325325Unknown Amount of Work, 25°C (77°F)
Timken Test 22700 g50.0 lbOK Load
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 163 °C325 °FSee Note 2.
Minimum Service Temperature, Air -18.0 °C-0.400 °FSee Note 1.
Flash Point 300 °C572 °FSee Note 3.
Dropping Point 232 °C450 °F
 
Descriptive Properties
ColorDark Brown
TextureTacky
Thickener, %10Lithium Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WTEXA274 / 77153

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.