MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Forplast POLYETHYLENE PEHD P 131 (CRBB) PE 80 Post-Consumer Recycled HDPE
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: PE grade code: High Density Polyethylene (Post-Consumer Recycled)

Stabilization recipe: Antacid, antioxidant thermostabilized processing aid, dispersing agent carbon black.

Application: Pipe and cable protection pipe, Extrusion, no pressure pipe.

Information provided by Forplast Srl.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 - 0.969 g/ccCompound; ISO 1183
Oxidative Induction Time (OIT) >= 10 min
@Temperature 210 °C
ISO 11357
Carbon Black Loading 2.0 %
Melt Flow 1.3 - 2.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
UNI 1133T
Ash <= 5.0 %ASTM D1603
Storage Temperature <= 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 28.0 MPa50mm/min; UNI 5819
Tensile Strength, Yield >= 20.0 MPa50mm/min; UNI 5819
Elongation at Break >= 600 %50mm/min; UNI 5819
Modulus of Elasticity >= 0.700 GPaUNI EN ISO 527-2
 
Descriptive Properties
PP Content<5%
Supply formPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFORP904 / 316415

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.