MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Saflex® Medium Bronze Colored Protective Interlayer PVB Film for Glass Laminates
Categories: Polymer; Film; Thermoplastic

Material Notes: Saflex interlayers enhance the safety and UV protection in architectural glazing.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 65 %Solar
 69 %Visible
 
Descriptive Properties
Light to Solar Gain0.94
Relative Heat Gain181 BTU/h-ft2-°F
Shading Coefficient0.84
Solar Heat Gain Coefficient0.73
U factor1.01 BTU/h-ft2-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Saflex® PS41 PVB Encapsulant Silver Migration Formulation
Eastman Saflex® Medium Neutral Brown Colored Protective Interlayer PVB Film for Glass Laminates
Eastman Saflex® Medium Blue Grey Colored Protective Interlayer PVB Film for Glass Laminates
Eastman Saflex® Light Sky Blue Colored Protective Interlayer PVB Film for Glass Laminates
Eastman Saflex® HP 0.100 inch Clear Protective Interlayer PVB Film for Glass Laminates

PEAT7078 / 183646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.