  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ovako 16MNCrS5, 4306 (M) Steel, +A, Round bar
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: 16MnCr5(M) is a grade with improved machinability. It is recommended for applications with high demands on mechanical properties, machinability and surface quality. It is also suitable for case hardening and has good weldability.

Information provided by Ovako

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 150
@Thickness 25.0 - 160 mm
<= 150
@Thickness 0.984 - 6.30 in
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 418 °C784 °FMS
 738 °C1360 °FAC1
 738 °C1360 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.0050 - 0.050 %0.0050 - 0.050 %
Carbon, C 0.14 - 0.18 %0.14 - 0.18 %
Chromium, Cr 0.80 - 1.1 %0.80 - 1.1 %
Iron, Fe 96.86 - 97.94 %96.86 - 97.94 %As Balance
Manganese, Mn 1.0 - 1.35 %1.0 - 1.35 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 0.10 - 0.40 %0.10 - 0.40 %
Sulfur, S 0.020 - 0.040 %0.020 - 0.040 %
 
Descriptive Properties
WeldabilityCEV 0.59max
 Pcm 0.29max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1095 Steel, oil quenched from 800°C (1475°F), tempered at 540°C (1000°F)
AISI 1095 Steel, oil quenched from 800°C (1475°F), tempered at 480°C (900°F)
AISI 1095 Steel, as rolled
AISI 1095 Steel, annealed at 790°C (1450°F)
ASTM A500 Steel, grade C, shaped structural tubing

NOVAKO084 / 234383

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.