MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Excel Industries DETC O,O-Diethylthiophosphoryl Chloride
Categories: Other Engineering Material

Material Notes: CSA No: 2524-04-01

O,O-Diethyldithophosphoric Chloride (DETC) is the intermediate used in the manufacture of many Organophosphorus pesticides.

Applications:

  • It is used as an intermediate in the manufacture of many Organophosphorus pesticides like: Quinalphos, Chlorphyriphos,. Triazophos, Diazinon, Demeton, Profenophos.
  • It is also used in the manufacture of Corrosion inhibitors, Rubber accelerators, Floating agents, Oil additives, Gasoline additives and Plasticizers.

Information provided by Excel Industries Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.186 - 1.20 g/cc
@Temperature 25.0 °C
1.186 - 1.20 g/cc
@Temperature 77.0 °F
Molecular Weight 188.6 g/mol188.6 g/mol
 
Thermal PropertiesMetricEnglishComments
Boiling Point  71.0 - 72.0 °C
@Pressure 0.000933 MPa
160 - 162 °F
@Pressure 0.135 psi
 81.0 - 82.0 °C
@Pressure 0.00160 MPa
178 - 180 °F
@Pressure 0.232 psi
 96.0 - 98.0 °C
@Pressure 0.00333 MPa
205 - 208 °F
@Pressure 0.483 psi
 
Descriptive Properties
Physical stateColorless to light yellow fuming liquid
Purity>99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEXCEL004 / 183480

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.