MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyarylamide (PAA); Polyarylamide, Glass Fiber Filled

Material Notes: The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.

Data provided by the manufacturer, Solvay Advanced Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccdry as molded
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 70.0 MPaASTM D638
Elongation at Break 1.6 %ASTM D638
Tensile Modulus 6.50 GPaASTM D638
Flexural Yield Strength 120 MPaASTM D790
Flexural Modulus 5.50 GPaASTM D790
Izod Impact, Notched 0.350 J/cmASTM D256
Izod Impact, Unnotched 2.50 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 °C
 
Processing PropertiesOriginal ValueComments
Feed Temperature 250 - 280 °C
Rear Barrel Temperature 250 - 280 °CCompression Zone
Middle Barrel Temperature 250 - 280 °CHomogenization Zone
Front Barrel Temperature 260 - 290 °CNozzle Zone
Melt Temperature 280 °C
Mold Temperature 120 - 140 °CNeeded to develop high crystallinity
Injection Pressure 50.0 - 250 MPa
Hold Pressure 30.0 - 150 MPa
Back Pressure 0.000 - 1.00 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
RTP Company RTP 207 K Polyarylamide (PAA), Glass Fiber
RTP Company RTP 205 K Polyarylamide (PAA), Glass Fiber
RTP Company RTP 0299 K X 138337 E Polyarylamide (PAA); Flame Retardant - Glass Fiber - Low Warp
Lehvoss LUVOCOM® 16-8960/ES Polyarylamide with carbon fiber and steel fiber

PSOLO1 / 68335

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.