MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded; Medium Density (MDPE)

Material Notes: Features: Excellent ESCR and toughness, high strength, excellent processability.

Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.

Data provided by the manufacturer.

Key Words: Medium Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
ESCR 100% Igepal® >= 5000 hour>= 5000 hourF0, Condition C, ASTM D1693
Melt Flow 0.14 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.14 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Ultimate 31.0 MPa4500 psiASTM D638
Tensile Strength, Yield 20.0 MPa2900 psiASTM D638
Elongation at Break 800 %800 %ASTM D638
Tensile Modulus 0.800 GPa116 ksiSecant; ASTM D638
Flexural Modulus 0.780 GPa113 ksiSecant; ASTM D3350
 
Thermal PropertiesMetricEnglishComments
CTE, linear 140 µm/m-°C
@Temperature 20.0 °C
77.8 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 128 °C262 °FASTM D3417
Vicat Softening Point 119 °C246 °FASTM D1525
Brittleness Temperature <= -100 °C<= -148 °FASTM D696
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 - 225 °C383 - 437 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade
Total Finathene® 3344N Natural HDPE pipe grade
Total HP 401 MDPE, pipe, cable, sheet
Ineos G50-100 HDPE
LyondellBasell Petrothene® LP500200 High Density Polyethylene (Sheet & Profile Grade)

PEHN2S / 35613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.