MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® X PS-154200101 WHITE Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D792
Filler Content 30 %30 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
@Thickness 3.18 mm
0.0030 - 0.0060 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.013 - 0.022 cm/cm
@Thickness 3.18 mm
0.013 - 0.022 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 82.7 MPa12000 psi5.1 mm/min; ASTM D638
Elongation at Break 3.0 - 5.0 %3.0 - 5.0 %ASTM D638
Tensile Modulus 6.89 GPa999 ksi5.1 mm/min; ASTM D638
Flexural Strength 134 MPa19400 psi1.3 mm/min; ASTM D790
Flexural Modulus 6.62 GPa960 ksi1.3 mm/min; ASTM D790
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °FUnannealed; ASTM D648
 
Descriptive Properties
FeaturesGood Chemical Resistance
 High Heat Resistance
 Impact Modified
 Semi Crystalline
FormsPellets
Generic MaterialPBT
Generic NamePolybutylene Terephthalate (PBT)
Regional AvailabilityNorth America
 South America
UsesAppliance Components
 Appliances
 Automotive Applications
 Consumer Applications
 Housings
 Industrial Applications
 Sporting Goods
 Structural Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced
Celanese Celanex® 1400A PBT, Unfilled
Avient Trilliant™ HC HC3320-0020 RS Natural Polybutylene Terephthalate (PBT)
Celanese Celanex® 1400FC PBT, Unfilled
Celanese Celanex® 2401 MT PBT, Medical Technology

PH0POL1247 / 145816

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.