MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTAPEEK® MG red Medical Grade PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Product characteristics:
  • High purity
  • Very good sterilization resistance
  • ISO 10993 tested on semi-finished product
Product applications:
  • Medical engineering
  • Pharmaceutical industry
  • Precision mechanics

Information provided by Röchling.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³DIN EN ISO 1183-1
Water Absorption 0.20 %0.20 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888DIN EN ISO 868
Tensile Strength, Yield 110 MPa16000 psiDIN EN ISO 527
Elongation at Break 15 %15 %DIN EN ISO 527
Modulus of Elasticity 4.00 GPa580 ksiDIN EN ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.90e+16 ohm-cm4.90e+16 ohm-cmDIN EN 62631-3-1
Surface Resistance 1.00e+18 ohm1.00e+18 ohmDIN EN 62631-3-2
Dielectric Constant 3.23.2IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243
Dissipation Factor 0.0010
@Frequency 50 Hz
0.0010
@Frequency 50 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C27.8 µin/in-°FDIN 53752
Specific Heat Capacity 1.34 J/g-°C0.320 BTU/lb-°FDIN 52612
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 343 °C649 °FISO 11357-3
Maximum Service Temperature, Air 250 °C482 °Flong term
 310 °C590 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 152 °C306 °FDIN EN ISO 75
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Moplen EP336J Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP300C Polypropylene, Impact Modified; Molded/Extruded
Aclo Accutech Polypropylene Homopolymer HP0334C10L Calcium Reinforced

PROCH9328 / 233030

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.