PH 0130 is a low melt flow rate homopolymer with a general purpose additive package. This resin is designed for blow molding and extrusion. PH 0130 features excellent processability and stiffness/impact strength balance. Its applications include: bottles for mineral water, drinks, and cosmetics; general use; ropes; flat and corrugated sheets; profiles; tear tape; and tapes in general. |