MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lushan PA+30% GF+5% AR-1A Nylon Toughener/PA Impact Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyolefin

Material Notes: Nylon toughener/PA impact modifier Lushan series is a maleic anhydride grafted polyolefin elastomer, with a very low residual maleic anhydride monomer, no irritating odor when using. Nylon toughener/PA impact modifier Lushan series has good response compatibility, elastomer dispersed in PA matrix rapidly to form the fine dispersed elastomer phase and the combined closely two-phase interface structure. Consequently, thereby Nylon thoughener/PA impact modifier Lushan series can be used for enhancing the toughness of nylon, and improving the impact resistant of the finished articles.

Nylon Toughener Usage:

  • 1. As impact modifier for toughening Nylon products like PA6, PA66, etc. To improve the impact resistance, lower water absorption of nylon products:
  • 2. As compatibilizer for PA/PE, PA/PP alloy.

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Index of Compound 1.0 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 139 MPa
Elongation at Break 28 %
Flexural Strength 154 MPa
Izod Impact, Notched (ISO) 19.5 kJ/m²

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BNZ Materials PA 20 Insulating Firebrick
AGC Fluon® PA1015Z 15% Glass Fiber, PTFE Filled Compound
Protactinium, Pa
RTP Company RTP PA6 30 GF BLK Nylon 6 (PA), Value Product - Glass Fiber - Heat Stabilized
Aclo Accutech Polypropylene CP0437T40V Copolymer Talc Reinforced

PLUSH036 / 150034

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.