Slack wax is a mixture of oil & wax, obtained from lubricating oil. Slack wax is the crude wax produced by chilling and solvent filter-pressing wax distillate. It serves as feedstock and that is further and blended to create value added petroleum wax products.Information provided by Ganpati Exim PVT. LTD. |