MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon T3015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Side 1: Cured Fusible Silicone Rubber
Substrate: 25% Sinusoidal Fiberglass
Side 2: Cured Fusible Silicone Rubber
Interleave: Polyester Film

Arlon MOX-Tape® Fiberglass Reinforced Tape: These self-fusing silicone rubber tapes incorporate a sinusoidal fiberglass fabric that gives a controlled elongation and increased tear resistance. This reinforcement provides excellent mechanical characteristics white allowing the tape to conform to irregular shapes.

Performance Advantages:
Resists moisture, oxygen, and ozone to assure continuous high insulation values.
Conforms smoothly when wrapped around complex forms.
Bonds to itself at room temperature within 24 hours.
Remains non-tacky to the touch and does not adhere to other surfaces, or substrates.
Insulates with single wrap, thereby reducing labor time and cost.
Dampens vibration and resists heat and mechanical shock as well as corona.
Inherently flame resistant and when burned forms a non-conductive ash.
SA & SB MOX-Tapes® provide a uniform thickness even around sharp edges. Fiberglass fabric, encapsulated inside the silicone rubber, prevents wicking and maintains high insulation resistance under high humidity conditions. These controlled stretch tapes provide a uniform insulation barrier.
All tapes are protected by a special interleaved liner.

Applications:

    Mechanical:
  • Protection of coils from vibration.
  • Vibration fixture, anti-scratch, and clamping pads.
  • Harness wrapping and wire bundling, including for high temperature applications.
  • Applied to rollers for protection and traction.
  • Plant maintenance.
  • Superior, heavy duty repair tape for emergency insulating barrier.
    Electrical:
  • Insulation of field armature and interpole coils in large motors.
  • Insulation for splicing and terminating of wire and cable.
  • Insulating and sealing electrical connections.
  • Insulating coil leads and bus bar connections.
  • Electromagnetic coil insulation.
  • Motor connections.
  • Overwrapping of deteriorated insulation in reclaimed motors.
    Environmental:
  • On-board aviation and space applications.
  • Underground cable splices.
  • Insulating heated transfer lines.
  • Insulating in radioactive environments.
  • Masking agent utilized in manufacturing processes and powder coatings.
  • Insulating, protecting, and sealing rigging hardware and power systems in marine applications.

This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns1.00 milInterleave
 203 microns8.00 milSubstrate; Arlon SQA-TMS-012
 381 microns15.0 milOverall; Arlon SQA-TMS-012
 25400 microns1000 milWidth; Arlon SQA-TMS-012
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050Silicone Property; ASTM D2240
Tensile Strength 8.260 MPa1198 psiSilicone Property; ASTM D412
 28.03 MPa4066 psiProduct Property; Arlon SQA-TMS-048
Elongation at Break 28 %28 %Tape Property; Arlon SQA-TMS-048
 580 %580 %Silicone Property; ASTM D412
Tear Strength 21.7 kN/m124 pliDie B, Silicone Property; ASTM D624
Peel Strength 0.754 kN/m4.30 pliAdhesion Strength, Tape Property; Arlon SQA-TMS-047
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 22.2 kV/mm563 kV/inTape Property; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 21.1 °C
12.0 Month
@Temperature 70.0 °F
From date of manufacture
 
Descriptive Properties
ColorNaturally WhiteSubstrate
 Red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene
Syensqo (Solvay Specialty Polymers) RHODOLINE® WA 265 Surfactant
Solvay RHODAFAC® RE-610 E Surfactant
Rogers Arlon T4015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Rogers Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate

PARL684 / 125870

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.