MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zircar Ceramics AL-25/1700 Alumina Insulation
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: AL-25/1700 is a rigid medium duty grade of alumina fiber board. Not as strong as SALI but capable of delivering years of service.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.440 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00138 GPaParallel to Thickness
Compressive Yield Strength 35.0 psiat 2% Consolidation, Parallel to Thickness
 
Electrical PropertiesOriginal ValueComments
Dielectric Loss Index 0.010
@Frequency 2.45e+9 Hz,
Temperature 1400 °C
In Microwave
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.110 W/m-K
@Temperature 400 °C
parallel to thickness; ASTM C177-76
 0.160 W/m-K
@Temperature 800 °C
 0.220 W/m-K
@Temperature 1100 °C
 0.270 W/m-K
@Temperature 1650 °C
Parallel to Thickness; ASTM C177-76
Maximum Service Temperature, Air 1700 °CContinuous
Shrinkage 0.75 %
@Temperature 1700 °C,
Time 86400 sec
Length & Width
 3.0 %
@Temperature 1700 °C,
Time 86400 sec
Thickness
 
Component Elements PropertiesOriginal ValueComments
Al2O3 80 %
SiO2 20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Ceramics AL-30 Alumina Insulation
Zircar Ceramics AL-30AA Alumina Insulation
Zircar Ceramics AL-30AAH Alumina Insulation
Zircar Ceramics ECO-20AA Alumina Insulation
Zircar Ceramics SALI Alumina Insulation

CZIR044 / 2852

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.