MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Laminar Filler
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.

MILLATHANE® HT compounds need only three ingredients when curing with peroxide: MILLATHANE HT, stearic acid and peroxide. However, reinforcing fillers are necessary. Because without them, the tensile, elongation and tear properties of MILLATHANE HT compounds do not attain their maximum values. In comparison with sulfur cures, peroxide-cured compounds have superior compression set, faster cure times and better heat resistance. However, sulfur-cured compounds exhibit higher tensile and elongation characteristics.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5454
Tensile Strength 10.6 MPa1540 psi
Elongation at Break 426 %426 %
100% Modulus 1.79 MPa
@Strain 100 %
260 psi
@Strain 100 %
200% Modulus 2.94 MPa
@Strain 200 %
427 psi
@Strain 200 %
300% Modulus 4.56 MPa
@Strain 300 %
662 psi
@Strain 300 %
Tear Strength 26.4 kN/m151 pliDie C
Compression Set 57 %
@Temperature 70.0 °C,
Time 79200 sec
57 %
@Temperature 158 °F,
Time 22.0 hour
 
Processing PropertiesMetricEnglishComments
Cure Time 20.0 min
@Temperature 154 °C
0.333 hour
@Temperature 310 °F
Press cured
 
Descriptive Properties
Formulation as Tested0.5Zinc Stearate
 1THANECURE® ZM
 1.5Sulfur
 100Millathane HT
 2MBT
 20Laminar
 4MBTS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMILL320 / 87364

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.