MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Overview of materials for Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Cast Iron". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 5.54 - 7.81 g/ccAverage value: 7.23 g/cc Grade Count:143
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 110 - 807Average value: 300 Grade Count:156
Hardness, Knoop 162 - 906Average value: 288 Grade Count:78
Hardness, Rockwell B 40.0 - 97.0Average value: 69.3 Grade Count:4
Hardness, Rockwell C 11.4 - 65.0Average value: 30.9 Grade Count:45
Hardness, Vickers 151 - 871Average value: 273 Grade Count:78
Tensile Strength, Ultimate 90.0 - 1650 MPaAverage value: 496 MPa Grade Count:160
Tensile Strength, Yield 65.5 - 1450 MPaAverage value: 426 MPa Grade Count:114
Elongation at Break 0.200 - 40.0 %Average value: 7.98 % Grade Count:103
Reduction of Area 2.00 - 10.0 %Average value: 5.38 % Grade Count:13
Modulus of Elasticity 62.1 - 250 GPaAverage value: 147 GPa Grade Count:64
Flexural Yield Strength 248 - 655 MPaAverage value: 496 MPa Grade Count:9
Compressive Yield Strength 220 - 2520 MPaAverage value: 987 MPa Grade Count:39
Poissons Ratio 0.240 - 0.370Average value: 0.286 Grade Count:37
Fatigue Strength 68.9 - 510 MPaAverage value: 260 MPa Grade Count:31
Fracture Toughness 44.0 - 110 MPa-m½Average value: 81.4 MPa-m½ Grade Count:7
Machinability 0.000 - 125 %Average value: 39.0 % Grade Count:10
Shear Modulus 27.0 - 67.6 GPaAverage value: 58.4 GPa Grade Count:36
Shear Strength 149 - 1480 MPaAverage value: 528 MPa Grade Count:28
Izod Impact Unnotched 4.00 - 244 JAverage value: 65.5 J Grade Count:12
Charpy Impact 0.100 - 40.0 JAverage value: 16.7 J Grade Count:14
Charpy Impact, Unnotched 2.70 - 200 JAverage value: 72.4 J Grade Count:26
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000500 - 110 ohm-cmAverage value: 6.11 ohm-cm Grade Count:18
Magnetic Permeability 100 - 750Average value: 410 Grade Count:5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.75 - 19.3 µm/m-°CAverage value: 12.8 µm/m-°C Grade Count:30
Specific Heat Capacity 0.506 J/g-°CAverage value: 0.506 J/g-°C Grade Count:3
Thermal Conductivity 8.50 - 53.3 W/m-KAverage value: 26.9 W/m-K Grade Count:25
Melting Point 1120 - 1430 °CAverage value: 1190 °C Grade Count:9
Solidus 1140 - 1270 °CAverage value: 1220 °C Grade Count:3
Liquidus 1220 - 1430 °CAverage value: 1320 °C Grade Count:3
Maximum Service Temperature, Air 649 - 982 °CAverage value: 720 °C Grade Count:9
Minimum Service Temperature, Air -59.4 - -30.0 °CAverage value: -34.9 °C Grade Count:6
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.0500 - 25.0 %Average value: 3.26 % Grade Count:7
Antimony, Sb 0.00200 - 0.200 %Average value: 0.0174 % Grade Count:7
Arsenic, As 0.0200 %Average value: 0.0200 % Grade Count:6
Bismuth, Bi 0.00200 %Average value: 0.00200 % Grade Count:6
Boron, B 0.000600 %Average value: 0.000600 % Grade Count:6
Cadmium, Cd 0.00500 %Average value: 0.00500 % Grade Count:6
Carbon, C 0.400 - 4.10 %Average value: 3.13 % Grade Count:146
Cerium, Ce 0.00500 - 0.200 %Average value: 0.102 % Grade Count:24
Chromium, Cr 0.0300 - 35.0 %Average value: 3.82 % Grade Count:94
Copper, Cu 0.000 - 10.0 %Average value: 0.994 % Grade Count:75
Iron, Fe 49.0 - 96.3 %Average value: 86.9 % Grade Count:153
Lead, Pb 0.00200 - 0.00300 %Average value: 0.00214 % Grade Count:7
Magnesium, Mg 0.0200 - 0.0700 %Average value: 0.0450 % Grade Count:36
Manganese, Mn 0.100 - 4.50 %Average value: 0.739 % Grade Count:141
Molybdenum, Mo 0.000 - 16.0 %Average value: 0.797 % Grade Count:86
Nickel, Ni 0.000 - 43.0 %Average value: 6.35 % Grade Count:93
Oxygen, O 0.00500 %Average value: 0.00500 % Grade Count:6
Phosphorus, P 0.00200 - 1.00 %Average value: 0.0888 % Grade Count:131
Selenium, Se 0.0300 %Average value: 0.0300 % Grade Count:6
Silicon, Si 0.300 - 17.0 %Average value: 2.33 % Grade Count:154
Sulfur, S 0.00200 - 0.250 %Average value: 0.0698 % Grade Count:118
Tellurium, Te 0.0200 %Average value: 0.0200 % Grade Count:6
Tin, Sn 0.0100 - 0.300 %Average value: 0.0538 % Grade Count:12
Titanium, Ti 0.0400 %Average value: 0.0400 % Grade Count:6
Vanadium, V 0.100 - 2.00 %Average value: 0.478 % Grade Count:9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Alloy Cast Iron
Gray Cast Iron, ASTM A 48 Class 40
Overview of materials for Stainless Steel
Overview of materials for Gray Cast Iron
Overview of materials for High Carbon Steel

M01012 / 81703

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.