MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Arcol® F-3222 Polyol
Categories: Polymer; Thermoset

Material Notes: Characterization: Arcol F-3222 polyol is a 3,200-molecular-weight triol used in the production of one-shot flexible urethane slabstock foams.

Properties / Applications: Arcol F-3222 polyol is a 3,200-molecular-weight triol used in the production of one-shot flexible urethane slabstock foams. The full range of flexible foams from extra super soft to extra firm, with varying densities, can be made with Arcol F-3222 polyol. It provides an optimized balance of foam hardness, mechanical properties and processing ease, while maintaining yields. As with any product, use of Arcol F-3222 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Bulk Density 1.03 g/cc0.0372 lb/in³
Viscosity 520 cP520 cP
Storage Temperature 15.0 - 60.0 °C59.0 - 140 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.020<= 0.020[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 200 °C>= 392 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<50 APHA
Hydroxyl number50.5-53.5 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Arcol® F-1080 Polyol
Covestro Arcol® F-3040 Polyol
Covestro Arcol® F-3022 Polyol
Covestro Arcol® F-1522 Polyether Polyol
Covestro Arcol® E-919 Polyether Polyol

PCOVEST0025 / 201808

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.