MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem Taipol® SBR-1712E Styrene-Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Product Description: Taipol SBR-1712E is an emulsion styrene-butadiene rubber produced by cold polymerization using mixed acid soap as emulsifiers, acid coagulant, stabilized by a staining antioxidant and is extended with 37.5 parts of highly aromatic oil. SBR-1712E exhibits superior processing properties with extender oil, good wear, tear, abrasion and cracking resistance.

Applications: Taipol SBR-1712E finds use in tires, footwear, conveyor belts, camelback, automotive products, seals, wire & cable, molded and extruded industrial goods where color and staining are not major concern.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 42 - 56
@Temperature 100 °C
(1+4), Raw Polymer
Ash <= 1.0 %
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22.5 - 24.5 %Bound
 
Descriptive Properties
StabilizerStaining

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH210 / 315128

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.