MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® S5225 Two-Component Easy Mix Ratio Encapsulant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Primarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, thermal and mechanical shock resistance, and thermal conductivity.
  • Mix Ratio by weight = 100:100
  • Poor Chemical Resistance
  • Filled
  • Low Viscosity
  • High temperature
Cure Type: Room Temp or Heat Bonding Type: Silicone

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccMixed
Brookfield Viscosity 2230 cP50 rpm
 2420 cPMixed; 50 rpm
 2550 cPPart B; 50 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+13 ohm-cm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
Dielectric Strength 17.7 kV/mm
Dissipation Factor 0.010
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 220 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg -120 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 150 °C
Option 3. Post cure of 1 hour at 100ºC recommended
 1.00 hour
@Temperature 100 °C
Option 2, Post cure of 1 hour at 100ºC is recommended.
 16.0 hour
@Temperature 25.0 °C
Option 1, For optimum performance, follow the initial cure with a post cure of 1 hour at 100ºC.
Working Life 240 min
@Temperature 25.0 °C
100 g
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceBlackPart B
 GrayCured
 Off WhitePart A
Mix Ratio, by Volume100 : 100Part A : Part B
Mix Ratio, by Weight100 : 100Part A : Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil CV3-2640 Silicone, Conductive/Static Dissipative
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
Momentive Performance Materials RTV658B Low Volatile Silicone Adhesive Sealant Component, Clear
Henkel Loctite® Nuva-Sil® 5092 Non-corrosive Potting
Henkel Loctite® 5071 Silicone Encapsulant

PEMERS34 / 35726

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.